Citrate or hydrotalcite? : As the precursor of Pt or Ru-doped Ni/Mg(Al)O catalyst for propane oxidative reforming |
|
言語 |
en |
作成者 |
Zhan, Yingying
Li, Dalin
Nishida, Kazufumi
Shishido, Tetsuya
Oumi, Yasunori
Sano, Tsuneji
Takehira, Katsuomi
|
アクセス権 |
|
|
アクセス権 |
open access |
|
アクセス権URI |
http://purl.org/coar/access_right/c_abf2 |
権利情報 |
|
|
権利情報 |
Copyright (c) 2009 Elsevier B.V. |
主題 |
|
|
主題Scheme |
Other |
|
主題 |
C3H8 reforming |
主題 |
|
|
主題Scheme |
Other |
|
主題 |
H2 production |
主題 |
|
|
主題Scheme |
Other |
|
主題 |
Pt or Ru-Ni/Mg(Al)O catalyst |
主題 |
|
|
主題Scheme |
Other |
|
主題 |
Citrate |
主題 |
|
|
主題Scheme |
Other |
|
主題 |
Hydrotalcite |
主題 |
|
|
主題Scheme |
NDC |
|
主題 |
570 |
内容記述 |
|
|
内容記述 |
Trace amounts of Pt- and Ru-doped Ni/Mg(Al)O catalysts were prepared by a citrate method and tested in the oxidative reforming of C3H8 under daily start-up and shut-down (DSS) operation. The activity and the sustainability of the catalysts were compared with those of the Pt- and Ru-doped Ni/Mg(Al)O catalysts derived from hydrotalcite (HT) precursor. The DSS operation of C3H8 reforming was carried Out with O-2 gas or O-2/H2O mixed gas between 200 degrees C and 600 degrees C or 700 degrees C under air purging conditions. The catalysts underwent steaming treatment with H-2/H2O mixed gas at 900 degrees C for 10 h. This allowed us to test the effect of Ni sintering on the catalyst deactivation. Coking was significantly suppressed on both HT- and citrate-derived Ni catalysts. Although both preparations produced highly dispersed Ni particles on the catalysts, the HT-derived catalysts exhibited more finely dispersed Ni particles, resulting in higher activity values than those of the citrate-derived catalysts, The regenerative activity due to redispersion of sintered Ni particles was enhanced over the HT-derived catalysts compared with the activity over citrate-derived catalysts. Although a clear redispersion of Ni particles was not observed in the oxidative reforming, i.e., in the absence of steam, the size decrease in Ni particles was more significant over the HT-derived catalysts than over the citrate-derived catalysts. The Mg(Al)O periclase structure derived from Mg-Al HT likely plays an important role in the regenerative activity of Pt- and Ru-Ni/Mg(Al)O catalysts. Pt-doping was more effective than Ru for the catalyst sustainability in the oxidative reforming of C3H8. |
|
言語 |
en |
出版者 |
|
|
出版者 |
Elsevier Science BV |
言語 |
|
|
言語 |
eng |
資源タイプ |
|
|
資源タイプ識別子 |
http://purl.org/coar/resource_type/c_6501 |
|
資源タイプ |
journal article |
出版タイプ |
|
|
出版タイプ |
AO |
|
出版タイプResource |
http://purl.org/coar/version/c_b1a7d7d4d402bcce |
関連情報 |
|
|
|
識別子タイプ |
DOI |
|
|
関連識別子 |
10.1016/j.apcata.2009.01.015 |
関連情報 |
|
|
|
識別子タイプ |
DOI |
|
|
関連識別子 |
http://dx.doi.org/10.1016/j.apcata.2009.01.015 |
収録物識別子 |
|
|
収録物識別子タイプ |
ISSN |
|
収録物識別子 |
0926-860X |
収録物識別子 |
|
|
収録物識別子タイプ |
NCID |
|
収録物識別子 |
AA10821202 |
開始ページ |
|
|
開始ページ |
231 |
書誌情報 |
Applied Catalysis A-Gdeneral
Applied Catalysis A-Gdeneral
巻 356,
号 2,
p. 231-242,
発行日 2009
|
旧ID |
27702 |